Researchers increase performance capabilities of lithium-sulfur cathode by 50%

Thu, 10/10/2019 - 15:37 -- Paul Crompton

Scientists from Singapore-based NanoBio Lab (NBL) have developed a means of making lithium-sulfur cathodes that increase specific energy and curbs capacity fade. 

The team began by building the carbon host before adding the sulfur source to obtain a 3D interconnected porous nanomaterial.